Polymer Property : Seal Strength = 2600 g/25 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Seal Strength 2600 g/25 mm
2600 g/in
Seal Bar Temp approx. 135-145°C
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se..
Seal Strength <= 2600 g/25 mm
<= 2600 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Seal Strength <= 2600 g/25 mm
<= 2600 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..
Seal Strength <= 2600 g/25 mm
<= 2600 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s..
Seal Strength <= 2600 g/25 mm
<= 2600 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces..
Seal Strength 2600 g/25 mm
2600 g/in
Seal Bar Temp approx. 140-150°C
DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,..