Mechanical Properties Metric English Comments
Seal Strength 156 g/25 mm
156 g/in
DuPont Teijin Films Mylar® M34 Polyester Film, 50 Gauge (13 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Seal Strength 156 g/25 mm
156 g/in
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Seal Strength 156 - 201 g/25 mm
156 - 201 g/in
Average value: 188 g/25 mm Grade Count:7
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum an..