Mechanical Properties Metric English Comments
Seal Strength >= 1400 g/25 mm
>= 1400 g/in
Exxon Method - Extrusion coating on a 8.9 cm coating line at 30 cm/s and melt temp. of 329°C
ExxonMobil Escorene® LD-203 LDPE Extrusion Coating for Milk Cartons, High Speed  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low density polyethylene resin with excellent adhesion, drawability and heat sealability. LD-203 also exhibits excellent barrier properties and g..
Seal Strength >= 1400 g/25 mm
>= 1400 g/in
Sentinel Sealer Test
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..
Seal Strength >= 1400 g/25 mm
>= 1400 g/in
Sentinel Sealer Test
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..
Seal Strength 1400 g/25 mm
1400 g/in
seal bar 140°C.
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol..
Seal Strength 1400 - 2700 g/25 mm
1400 - 2700 g/in
Average value: 2280 g/25 mm Grade Count:4
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m..
Seal Strength 1400 g/25 mm
1400 g/in
PP, bar temp 204°C
DuPont Appeel® LSR 2044 Modified EVA Lidding Sealing Resin
Appeel® 2044 is a blown or cast film resin designed to be a sealing layer for lidding applications. It provides a peelable seal over a broad temperature range to a number of container materials inc..