Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 430 MPa | 62400 psi | ASTM D 882 |
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
1% Secant Modulus, TD | 430 MPa | 62400 psi | ASTM-D882 |
Braskem LH537 LLDPE Cast Film Extrusion Polyethylene LH537 is a LLDPE Hexene produced by Braskem. It offers an excellent processability, stiffness, and soft touch for flat die films. It has very low gel contents. It contains slip absent and antiblock .. |
|||
1% Secant Modulus, TD | 430 MPa | 62300 psi | ASTM D882 |
ExxonMobil LL 3404.48 Cast Film Resin
(discontinued **) LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |