Polymer Property : 1% Secant Modulus, TD = 370 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 370 MPa
53700 psi
ISO 527-3
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene
Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco..
1% Secant Modulus, TD 370 MPa
53700 psi
ASTM D 882
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin
FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-..