Mechanical Properties Metric English Comments
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
ExxonMobil LL 3301.34 Premium High Strength Film Resin  (discontinued **)
LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi..
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
ExxonMobil LL 3301.63 Premium High Strength Film Resin  (discontinued **)
LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi..
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..
1% Secant Modulus, TD 238 MPa
34500 psi
ASTM D882
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene
ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene..