Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
LyondellBasell Petrothene® NA952000 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
LyondellBasell Petrothene® NA952094 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EB403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent shrinkability, and has very good optic.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EF923 Low Density Polyethylene Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
Westlake EN923 Low Density Polyethylene Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, TD | 221 MPa | 32000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
1% Secant Modulus, TD | 221 MPa @Thickness 0.0317 mm |
32000 psi @Thickness 0.00125 in |
ASTM D-882 |
Bapolene® 108A Low Density Polyethylene Film Extrusion Resin Bapolene® 108A is an LDPE for blown film. It contains 2500 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p.. |
|||
1% Secant Modulus, TD | 221 MPa @Thickness 0.0356 mm |
32000 psi @Thickness 0.00140 in |
ASTM D-882 |
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of .. |