Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, TD = 29000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 200 MPa
29000 psi
ISO 527-3
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain..
1% Secant Modulus, TD 200 MPa
29000 psi
ISO 527-3
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene
Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH ..
1% Secant Modulus, TD 200 MPa
29000 psi
ISO 527-3
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit..
1% Secant Modulus, TD 200 MPa
29000 psi
ISO 527-3
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
SABIC HP0722N Low Density Polyethylene for Blown Film
Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Westlake EF378 Low Density Polyethylene
WESTLAKE EF378 is suggested for cast film applications. It has excellent haze and gloss, good strength, good processability, and good heat sealability.Application/UsesDiaper linersGeneral purpose cl..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Westlake EF412 Low Density Polyethylene
WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Westlake EF421 Low Density Polyethylene
WESTLAKE polyethylene EF421 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and general purpose food packaging app..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin
Product Description: LGA 105 is a homopolymer, garment film resin with good toughness. It is capable of being draw-down to thin gauges.Availability: North America Additive: Antiblock: NoSlip: NoPro..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM-D882
Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer
LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM-D882
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene
LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM-D882
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains antiblock, proc..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These..
1% Secant Modulus, TD 200 MPa
29000 psi
ASTM D882
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene
Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing..
Copyright © lookpolymers.com All Rights Reserved