Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 261 MPa | 37800 psi | ASTM D882 |
ExxonMobil LL 1107x93 Blown Film Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||