Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1700 MPa
247000 psi
ASTM D882
SABIC F01552 High Density Polyethylene for Blown Film
Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
1% Secant Modulus, TD 1700 MPa
247000 psi
ASTM D882
SABIC F04660 High Density Polyethylene for Blown Film Applications
Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp..