Mechanical Properties Metric English Comments
1% Secant Modulus, TD 225.56 MPa
32714 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF1051 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF1051 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstandin..
1% Secant Modulus, TD 225.56 MPa
32714 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and ..
1% Secant Modulus, TD 225.56 MPa
32714 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene
LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..
1% Secant Modulus, TD 225.56 MPa
32714 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene
LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
1% Secant Modulus, TD 225.56 MPa
32714 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene
LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact ..