Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 306.38 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 306.57 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical |