Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | Blown; ASTM D882 |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | Blown; ASTM D882 |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM E111 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
Westlake Mxsten CV77518 Polyethylene Plastomer Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882, A |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
1% Secant Modulus, TD | 172 MPa @Thickness 0.0254 mm |
25000 psi @Thickness 0.00100 in |
ASTM D882A |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl.. |
|||
1% Secant Modulus, TD | 172 MPa | 24900 psi | ASTM D882 |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, TD | 172 MPa | 24900 psi | ASTM D882 |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, TD | 172 MPa | 24900 psi | ASTM D882 |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, TD | 172 MPa | 24900 psi | ASTM D882 |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: .. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade) Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa.. |
|||
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.56 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |