Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 96.5 MPa | 14000 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b.. |