Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 300 MPa | 43500 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex CL 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 508 exhibit a good bal.. |
|||
1% Secant Modulus, MD | 300 MPa | 43500 psi | ASTM D882 |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
1% Secant Modulus, MD | 300 MPa | 43500 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50.. |
|||
1% Secant Modulus, MD | 300 MPa | 43500 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid.. |
|||
1% Secant Modulus, MD | 300 MPa | 43500 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-.. |