Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 290 MPa | 42000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
1% Secant Modulus, MD | 290 MPa | 42000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
1% Secant Modulus, MD | 290 MPa | 42000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o.. |
|||
1% Secant Modulus, MD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr.. |
|||
1% Secant Modulus, MD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula.. |