Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 231 MPa | 33500 psi | ASTM D882 |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |