Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 186.32 MPa | 27024 psi | ASTM D882 |
Lotte Chemical Titan TITANLENE® LDF260YZ Low density polyethylene LDF260YZ is a low density polyethylene resin for film extrusion. LDF260YZ has no slip and anti-block additives. LDF260YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
1% Secant Modulus, MD | 186.32 MPa | 27024 psi | ASTM D882 |
Lotte Chemical Titan TITANLENE® LDF260GG Low density polyethylene LDF260GG is a low density polyethylene resin for film extrusion. LDF260GG has medium slip and anti-block additives. LDF260GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |