Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
LyondellBasell Petrothene® NA334000 Low Density Polyethylene ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
LyondellBasell Petrothene® NA350136 Low Density Polyethylene ApplicationsPETROTHENE NA 350-136 is a low density/EVA copolymer designed for heavy duty film packaging and other high strength, easy to seal packaging. NA 350-136 exhibits high impact strength and.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM E111 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
Westlake EF677 Low Density Polyethylene Westlake EF677 is a high melt index LDPE resin suggested for garment films, or other applications requiring excellent drawdown. This material is also an excellent choice for PE foam applications.App.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
Westlake LF2040 Hexene Linear Low Density Polyethylene Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
ExxonMobil LD 317.09 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
ExxonMobil LD 317.87 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM D882 |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |