Mechanical Properties Metric English Comments
1% Secant Modulus, MD 116 MPa
16800 psi
ASTM D 882
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin
FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou..