Mechanical Properties Metric English Comments
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin  (discontinued **)
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil ESCOR™ AT 310 Cast Film Resin  (discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
Westlake Mxsten CV77529 Polyethylene Plastomer
Mxsten CV plastomer CV77529 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil Escorene® LD 701.ID Blown Film Resin
Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin
Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin
Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
1% Secant Modulus, MD 110 MPa
16000 psi
ASTM D882
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the..