Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 97.1 MPa | 14100 psi | ASTM D790 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Flexural Yield Strength | 97.1 MPa @Thickness 3.20 mm |
14100 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® LW5300M PBT+PC+MF30% Description: Injection Molding, PBT+PC+MF30%, Low WarpageApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 103598-77-2, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 97.1 MPa @Thickness 3.20 mm |
14100 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC5004T PC/Polyester, Transparency Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 97.1 MPa @Thickness 3.20 mm |
14100 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |