Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 21.4 - 65.0 MPa | 3100 - 9430 psi | Average value: 37.8 MPa Grade Count:86 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Yield Strength | 22.0 - 65.0 MPa | 3190 - 9430 psi | Average value: 42.9 MPa Grade Count:15 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |