Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 59.8 MPa | 8680 psi | DIN 53455; ASTM D790 |
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Flexural Yield Strength | 59.8 MPa @Thickness 3.20 mm |
8680 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 59.8 MPa @Temperature 23.0 °C |
8680 psi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene AN450 Acrylonitrile Butadiene Styrene Applications:injection moldingelectric/electonic housing for microwave oven, tv, vcr, computer, etc. |