Polymer Property : Flexural Yield Strength = 86.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 86.3 MPa

@Thickness 3.20 mm
12500 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 86.3 MPa

@Thickness 6.40 mm
12500 psi

@Thickness 0.252 in
5mm/min; ASTM D790
LG Chemical Lupox® TE5000S PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided..
Flexural Yield Strength 86.3 MPa

@Thickness 3.20 mm
12500 psi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Flexural Yield Strength 86.3 MPa

@Thickness 3.20 mm
12500 psi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY HR5007AE PC/ABS, High Impact
Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 86.3 MPa

@Thickness 3.20 mm
12500 psi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY NS5000 PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 86.3 MPa
12500 psi
ASTM D790
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Flexural Yield Strength 86.3 MPa
12500 psi
ASTM D790
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Flexural Yield Strength 86.3 MPa
12500 psi
ASTM D790
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Flexural Yield Strength 86.3 MPa
12500 psi
ASTM D790
Samyang Trirex® 3026PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang.
Flexural Yield Strength 86.3 MPa
12500 psi
ASTM D790
Samyang Trirex® 3025A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Flexural Yield Strength 86.3 MPa
12500 psi
ASTM D790
Samyang Trirex® 3026B Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026B is an extrusion grade.Applications: BottlesInformation provided by Samyang.