Polymer Property : Flexural Yield Strength = 8180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 56.4 MPa

@Temperature 23.0 °C
8180 psi

@Temperature 73.4 °F
ASTM D790
IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets