Mechanical Properties Metric English Comments
Flexural Yield Strength 77.9 MPa
11300 psi
ASTM D790
Techmer ES Luriblend® POM HO TL20 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc.
Flexural Yield Strength 77.9 MPa
11300 psi
ASTM D790
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened
Data provided by Clariant Masterbatches
Flexural Yield Strength 77.9 MPa
11300 psi
ASTM D790
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened
Data provided by Clariant Masterbatches
Flexural Yield Strength 77.9 MPa
11300 psi
ASTM D790
PlastxWorld Veroplas PA2009L Nylon 6
general purpose, super lubricated injection molding gradeInformation provided by PlastxWorld Inc.
Flexural Yield Strength 77.9 - 207 MPa
11300 - 30000 psi
Average value: 109 MPa Grade Count:37
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..