Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.2 - 137 MPa | 11200 - 19900 psi | Average value: 110 MPa Grade Count:5 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech Spectar® Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 6120 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Albis Plastics ASA 02A MR20 , 20% Mineral Filled
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |