Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 74.5 MPa | 10800 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 74.5 MPa @Thickness 3.20 mm |
10800 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 74.5 MPa @Thickness 3.20 mm |
10800 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | ASTM-D790 |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Flexural Yield Strength | 74.5 MPa @Thickness 3.20 mm |
10800 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 74.5 MPa @Thickness 3.20 mm |
10800 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | ASTM D790 |
GRECO ISOPAK 547HF ABS Resin High Flow GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | 5% strain; ASTM D790 |
Metton LMR M1539 Liquid Molding Resin Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can .. |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | 5% strain; ASTM D790 |
Metton LMR M2100VO Liquid Molding Resin Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can .. |
|||
Flexural Yield Strength | 74.5 MPa @Thickness 3.20 mm |
10800 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR407E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by.. |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | ASTM D790 |
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | ASTM D790 |
Techmer ES Luriblend® POM CO E TL20 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance and CopolymerProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 74.5 MPa | 10800 psi | ASTM D790 |
PlastxWorld CEVIAN® S3100 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 74.5 - 220 MPa | 10800 - 31900 psi | Average value: 151 MPa Grade Count:46 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |