Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 73.55 MPa @Thickness 6.40 mm |
10670 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Yield Strength | 73.55 MPa @Thickness 6.40 mm |
10670 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-16M ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |