Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Flexural Yield Strength | 72.0 - 103 MPa | 10400 - 15000 psi | Average value: 89.2 MPa Grade Count:24 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | at 3.5% strain; 6.5% strain at break; ISO 178 |
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM-D790 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ISO 178 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific) Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® FS 2000 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosityAs of 1 S.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Kleerdex Kydex® 160 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Plaslok 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP CX94108 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CX94108 is a compound based on Polystyrene resin containing Proprietary Lubricant. Added features include: Internally Lubricated. |