Mechanical Properties Metric English Comments
Flexural Yield Strength 68.3 MPa
9910 psi
ASTM D790
Ineos ABS Lustran® Ultra 2337 General Purpose, Superhigh-Gloss  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..