Polymer Property : Flexural Yield Strength = 65.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 21.4 - 65.0 MPa
3100 - 9430 psi
Average value: 37.8 MPa Grade Count:86
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Flexural Yield Strength 22.0 - 65.0 MPa
3190 - 9430 psi
Average value: 42.9 MPa Grade Count:15
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..