Polymer Property : Flexural Yield Strength = 59.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 59.8 MPa
8680 psi
DIN 53455; ASTM D790
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
Flexural Yield Strength 59.8 MPa

@Thickness 3.20 mm
8680 psi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GP5008A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Flexural Yield Strength 59.8 MPa

@Temperature 23.0 °C
8680 psi

@Temperature 73.4 °F
ASTM D790
IRPC Polimaxx Porene AN450 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectric/electonic housing for microwave oven, tv, vcr, computer, etc.