Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 4980 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 34.3 MPa

@Thickness 6.40 mm
4980 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL EI5002L PP
Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical
Flexural Yield Strength 34.3 MPa
4980 psi
ASTM D790
KKPC Kuhmo HI 425 General Purpose HIPS
Key features: High-impact General Use. Common Uses: Office appliances, home appliances, various kitchenware, general merchandise, toys, leisure goods, etc.HIPS is a functional resin made by copolym..
Flexural Yield Strength 34.3 MPa
4980 psi
ASTM D790
KKPC Kuhmo HI 425TVL High Flow/High Heat Resistant HIPS
Key features: Super high-fluidity. Common Uses: TV cover (Fine TV), Drawers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-..
Flexural Yield Strength 34.3 MPa
4980 psi
ASTM D790
Samyang Trihip® B500 High Impact Polystyrene
Dimensional stability, electrical properties and weather resistance are excellent.B500 is the non-flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, P..
Flexural Yield Strength 34.3 MPa
4980 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 34.3 MPa
4980 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Copyright © lookpolymers.com All Rights Reserved