Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 48.1 MPa @Thickness 6.40 mm |
6970 psi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Flexural Yield Strength | 48.1 MPa @Thickness 6.40 mm |
6970 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 48.1 MPa @Thickness 6.40 mm |
6970 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade Antistatic Cop Sleeves ApplicationInformation provided by Bhansali |
|||
Flexural Yield Strength | 48.1 MPa @Thickness 6.40 mm |
6970 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade Antistatic Cop Sleeves ApplicationInformation provided by Bhansali |