Mechanical Properties Metric English Comments
Flexural Yield Strength 329 MPa

@Thickness 3.20 mm
47600 psi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Flexural Yield Strength 328 MPa
47600 psi
ASTM D790
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Flexural Yield Strength 328 MPa
47600 psi
ASTM D790
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..
Copyright © lookpolymers.com All Rights Reserved