Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 46.1 MPa @Thickness 3.20 mm |
6680 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Flexural Yield Strength | 46.1 MPa | 6680 psi | ASTM D790 |
IRPC Polimaxx Polene 2311KX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% TALCUM REINFORCED, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |