Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 45.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 45.5 - 221 MPa
6600 - 32000 psi
Average value: 172 MPa Grade Count:42
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet
Description: Weather Resistant SheetInformation provided by Spartech.
Flexural Yield Strength 45.5 MPa
6600 psi
Spartech Royalstatâ„¢ R671 ABS Static Control Sheet
Data provided by the manufacturer.
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 45.5 MPa
6600 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 5% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Copyright © lookpolymers.com All Rights Reserved