Mechanical Properties Metric English Comments
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
NYCOA 2084 HS PA 6
lubricated flexible tubing and conduitInformation provided by NYCOA, Inc.
Flexural Yield Strength 40.0 MPa
5800 psi
DIN 53452
Ineos Nova S-3400 Medium Impact Compact Polystyrene  (discontinued **)
Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. For injection molding generally a lubricated type is us..
Flexural Yield Strength 40.0 MPa
5800 psi
DIN 53452
Ineos Nova S-3401 Medium Impact Compact Polystyrene  (discontinued **)
Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. The material is provided with external lubricate to imp..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM Data
BASF Capron® 8202C HS Nylon 6 (Conditioned)  (discontinued **)
Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM Data
BASF Capron® 8203C HS Blend Nylon 6 (Conditioned)  (discontinued **)
Capron 8203C HS Blend is a heat stabilized, high viscosity nylon 6 extrusion compound possessing a modified crystalline structure for increased strength, stiffness and heat distortion temperature. ..
Flexural Yield Strength 40.0 MPa
5800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East)
LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated.
Flexural Yield Strength 40.0 MPa
5800 psi
ISO 178
Solvay Technyl® C 206 Nylon 6, EH50
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Spartech Litho SP-2090 Polystyrene Sheet
Description: Polystyrene SheetInformation provided by Spartech.
Flexural Yield Strength 40.0 MPa
5800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP
LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f..
Flexural Yield Strength 40.0 MPa
5800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP
LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Tipco Tipcolene® CR 8229 - 20% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology
20% Mineral Reinforced, High Flow & Controlled Rheology PP CopolymerApplications: Automotive Door TrimsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., I..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Tipco Tipcolene® FPT 30 PPC - 30% Talc Reinforced Polypropylene Copolymer Compound
30% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Tipco Tipcolene® FPT 20 PPC - 20% Talc Reinforced Polypropylene Copolymer Compound
20% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 40.0 MPa
5800 psi
2 mm/min; ASTM D790
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM Data
BASF Capron® 1202CQ Nylon 6 (Conditioned)  (discontinued **)
Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava..
Flexural Yield Strength 40.0 - 270 MPa

@Temperature -55.0 - 275 °C
5800 - 39200 psi

@Temperature -67.0 - 527 °F
Average value: 128 MPa Grade Count:8
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Flexural Yield Strength 40.0 MPa
5800 psi
DIN 53452
Ineos Nova S-3201 Medium Impact Compact Polystyrene  (discontinued **)
Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to ..
Flexural Yield Strength 40.0 - 1310 MPa
5800 - 190000 psi
Average value: 301 MPa Grade Count:31
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Flexural Yield Strength 40.0 MPa
5800 psi
ASTM D790
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 33% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..