Mechanical Properties Metric English Comments
Flexural Yield Strength 202 - 275 MPa
29300 - 39900 psi
Average value: 224 MPa Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Flexural Yield Strength 56.0 - 275 MPa
8120 - 39900 psi
Average value: 205 MPa Grade Count:24
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Flexural Yield Strength 131 - 275 MPa
19000 - 39900 psi
Average value: 160 MPa Grade Count:12
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Flexural Yield Strength 85.0 - 275 MPa

@Temperature -40.0 - 120 °C
12300 - 39900 psi

@Temperature -40.0 - 248 °F
Average value: 180 MPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..