Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 275 MPa | 39900 psi | ASTM D790 |
NYCOA 27/440KNF Glass Filled Nylon 6 44% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 275 MPa | 39900 psi | ASTM D790 |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Flexural Yield Strength | 275 MPa | 39900 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
Flexural Yield Strength | 275 MPa | 39900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Yield Strength | 275 MPa | 39900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LX04015 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LX04015 is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include: Electrically Conductive |
|||
Flexural Yield Strength | 275 MPa | 39900 psi | ASTM D790 |
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough.. |