Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 180 - 385 MPa | 26100 - 55800 psi | Average value: 262 MPa Grade Count:50 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 138 - 385 MPa | 20000 - 55800 psi | Average value: 216 MPa Grade Count:28 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |