Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 262 MPa | 38000 psi | ASTM D790 |
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 262 MPa | 38000 psi | ASTM D790 |
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 262 MPa | 38000 psi | ASTM D790 |
Clariant Renol PA111G33 Nylon 66, 33% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 262 MPa | 38000 psi | ASTM D790 |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 262 MPa | 38000 psi | ASTM D790 |
Chem Polymer Chemlon 143 G Nylon 66, 43% Glass Fiber Reinforced A 43% glass fiber reinforced nylon 66 offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 262 MPa | 38000 psi | ASTM D790 |
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |