Polymer Property : Flexural Yield Strength = 36800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 254 MPa
36800 psi
Conditioned; ASTM D790
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
Flexural Yield Strength 254 MPa
36800 psi
ASTM D790
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
Flexural Yield Strength 254 MPa
36800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Flexural Yield Strength 254 MPa
36800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Flexural Yield Strength 254 MPa
36800 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..