Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 245 MPa | 35500 psi | ASTM D790 |
NYCOA 27/300I Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 245 MPa | 35500 psi | ASTM Data |
BASF Capron® SEG6 H1 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG6 H1 is a 30% glass reinforced nylon 6 injection molding compound. This material is currently under development as XA-2678. It exhibits exceptional surface aesthetics at the slower fill s.. |
|||
Flexural Yield Strength | 245 MPa | 35500 psi | ASTM D790 |
Techmer ES Plaslube® J-1/30/TF/10 Nylon 66, 30% GFR, 10% PTFE Plaslube glass fiber reinforced, polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer an excellent balance of wear and friction performance and mechanical strength. The addition of silic.. |