Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 32.4 MPa @Thickness 6.40 mm |
4690 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HM3207SM PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, Good Weatherability, High ImpactApplication: Automotive Interior Parts CAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 32.4 MPa @Thickness 6.40 mm |
4690 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HM5302W PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 32.4 MPa | 4700 psi | ASTM D790 |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 32.4 MPa | 4690 psi | ASTM D790 |
Samyang Trihip® B300 High Impact Polystyrene, Flame Retardant Dimensional stability, electrical properties and weather resistance are excellent.B300 is the flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Print.. |