Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Yield Strength | 31.7 MPa | 4600 psi | Test specimens were injection molded by ASTM D1897; ASTM D790 |
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on f.. |
|||
Flexural Yield Strength | 31.7 MPa | 4600 psi | ASTM D790 |
Chevron Phillips K-Resin® BK10 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: BK10 is an SBC developed specifically to have enhanced flow capabilities. It offers improved processability and lower cycle times with the optical clar.. |