Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 306 MPa | 44400 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
Flexural Yield Strength | 306 MPa | 44400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |