Polymer Property : Flexural Yield Strength = 28100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 194 MPa
28100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Europe-Africa-Middle East)
LNP* STATKON* DEL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
Flexural Yield Strength 194 MPa
28100 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA
GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves.
Flexural Yield Strength 194 MPa
28100 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA (Asia Pacific)
GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves.
Flexural Yield Strength 194 MPa
28100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Flexural Yield Strength 194 MPa
28100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific)
LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat.
Flexural Yield Strength 194 MPa
28100 psi
2 mm/min; ISO 178
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded
Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar.